FIELD: metallurgy.
SUBSTANCE: grinding bodies are made of low-alloyed white iron, containing, wt %: C 3.2-3.6, Si 1.2-1.8, Cr 0.8-1.2, Mn 0.3-0.8, Ni 0.3-0.4, S <0.15, P <0.15, Fe - the rest.
EFFECT: production of grinding bodies, having simultaneously increased impact and wear resistance, when working under impact and abrasive wear.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING WEAR-RESISTANT WHITE IRON | 2009 |
|
RU2412780C1 |
CAST-IRON | 1999 |
|
RU2146300C1 |
CAST IRON | 0 |
|
SU1120030A1 |
METHOD FOR MANUFACTURE OF PIG IRON GRINDING BODIES | 1992 |
|
RU2016077C1 |
MILLING MEDIUM MANUFACTURED FROM HIGH CARBON STEEL OR CAST IRON, AND METHOD FOR MANUFACTURING THE SAME | 2002 |
|
RU2292240C2 |
CAST IRON FOR GRINDING BODIES | 1998 |
|
RU2128238C1 |
WEAR RESISTANT CAST IRON | 0 |
|
SU1068530A1 |
WHITE CAST IRON FOR THE MILLING BODIES | 0 |
|
SU1715876A1 |
WEAR RESISTANT CAST IRON | 2009 |
|
RU2384641C1 |
CAST IRON | 0 |
|
SU785376A1 |
Authors
Dates
2017-08-10—Published
2015-11-09—Filed