FIELD: chemistry.
SUBSTANCE: charge includes, wt %: liquid glass 9.2-9.8; sodium fluorosilicate 0.3-0.5; quartzite 20.5-22.0; iron scale 3.0-4.0; carborundum 3.9-4.7; dinas - the rest.
EFFECT: increasing the heat resistance of the refractory material.
1 tbl