FIELD: technological processes.
SUBSTANCE: method of applying decorative enamel to the products of amber is characterized by the fact that at the heart of amber product a recess is carved along the area of future figure, the depth of 0.5-1 mm, then the enamel of cold chemical curing is poured into the cut recess on the amber plate and placed in a muffle furnace heated to a temperature of 40-80°C, with a holding time of 4-24 hours, depending on the composition, layer thickness and enamel colour, or light-curing enamel is pour, and is stand under ultraviolet radiation with a wavelength of 195-480 nm, with a holding time of 2-10 minutes, depending on the composition, layer thickness and enamel colour.
EFFECT: obtaining decorative effect from connection of decorative product from amber with applied enamel, adjusting transparency and colour of received products.
1 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR DECORATING OF AMBER ARTICLE WITH ENAMEL | 2006 |
|
RU2314934C1 |
METHOD OF OBTAINING IMAGES ON AN ENAMEL SURFACE WITH A DEPTH EFFECT | 2018 |
|
RU2700897C1 |
METHOD FOR PRODUCTION OF MOSAIC OF ENAMEL GRANULATION | 2021 |
|
RU2785795C2 |
METHOD TO MAKE DECORATIVE ITEMS WITH FILLER FROM AMBER AND/OR WASTES OF ITS PROCESSING (VERSIONS) | 2010 |
|
RU2452715C1 |
METHOD OF MAKING DECORATIVE ARTICLES USING AMBER | 2011 |
|
RU2475366C1 |
METHOD OF MANUFACTURE OF INSERTIONS TO JEWELRY (VERSIONS) | 2010 |
|
RU2444967C1 |
METHOD OF PRODUCING AMBER PANEL | 2004 |
|
RU2279985C2 |
COATING ON THE ROLLED STEEL APPLICATION METHOD | 2017 |
|
RU2655984C1 |
METHOD OF PRODUCING COLOR PAINTING ON ENAMEL SURFACE | 2018 |
|
RU2695404C1 |
METHOD OF OBTAINING COLOURED DECORATIVE COATING ON TECHNICAL FABRIC FOR EXPLOITATION UNDER OUTER SPACE CONDITIONS | 2013 |
|
RU2533139C1 |
Authors
Dates
2017-10-11—Published
2015-10-20—Filed