FIELD: construction.
SUBSTANCE: implementation version of the present invention includes a settable composition containing ground non-expanded pearlite, pumicite, cement kiln dust, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, the ground non-expanded pearlite having an average particle size from about 1 mcm to about 100 mcm, cement kiln dust, the ground mixture of cement and pumicite, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, cement kiln dust, pumicite, and functional additives. The invention is developed in the dependent claims of the invention formula.
EFFECT: increased efficiency of cementing.
20 cl, 6 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
SETTING COMPOSITION CONTAINING NON-EXPANDED PEARLITE AND METHOD OF CEMENTING IN UNDERGROUND FORMATIONS | 2011 |
|
RU2599744C1 |
SETTABLE COMPOSITIONS COMPRISING UNEXPENDED PEARLITE AND METHODS OF CEMENTING IN UNDERGROUND FORMATIONS | 2011 |
|
RU2562627C2 |
CURABLE COMPOSITIONS CONTAINING CO-MILLED PEARLITE AND HYDRAULIC CEMENT | 2012 |
|
RU2584431C2 |
COMPACTING SPACER FLUIDS AND METHODS FOR USE THEREOF | 2013 |
|
RU2612763C2 |
PLACING A FLUID COMPRISING KILN DUST IN A WELLBORE THROUGH A BOTTOM HOLE ASSEMBLY | 2014 |
|
RU2657276C1 |
SOLIDIFYING COMPOSITIONS CONTAINING NATURAL PUZZOLANA AND METHOD RELATED THEREWITH | 2010 |
|
RU2507379C2 |
CURABLE COMPOSITIONS CONTAINING WOLLASTONITE AND PUMICE AND METHODS FOR USE THEREOF | 2013 |
|
RU2597906C1 |
METHODS AND COMPOSITIONS CONTAINING DUST OF A CEMENT-FURNACE WITH A CHANGED PARTICLE SIZE | 2013 |
|
RU2617493C2 |
METHOD OF BOREHOLE CEMENTATION | 2006 |
|
RU2404143C2 |
METHOD TO USE COMPOSITIONS INCLUDING CEMENT KILN DUST AND CAPABLE OF SETTING | 2006 |
|
RU2460870C2 |
Authors
Dates
2017-12-06—Published
2011-12-21—Filed