FIELD: construction materials.
SUBSTANCE: invention relates to construction materials and can be used for protection of various surfaces. Raw mixture for a protective coating contains, wt %: portland cement 39.18–41.20; fraction of sand 0.30 mm 32.39–32.79; micro calcite CaCO3 with a particle size of 100 microns 7.80–8.20; bentonite clay with a specific surface of 100,000 m2/kg 0.72–0.82; a complex additive 0.86–0.98; water 17.03–18.03. Complex additive contains, wt %: a redispersible powder based on styrene-acrylate copolymer Acronal 430 47.0–52.0; iron hydroxide sol with a density of ρ = 1.107 g/cm3 and pH = 9 48.0–53.0.
EFFECT: technical result is a decrease in abrasion (by 38 %) and a decrease in shrinkage of the protective coating (by 43 %).
1 cl, 1 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR PROTECTIVE COATING | 2018 |
|
RU2674779C1 |
RAW MIXTURE FOR PROTECTIVE COATING | 2018 |
|
RU2675390C1 |
RAW MIXTURE FOR PROTECTIVE COATING | 2023 |
|
RU2801566C1 |
CRUDE MIXTURE FOR PROTECTIVE COATING | 2019 |
|
RU2720170C1 |
CRUDE MIXTURE FOR PROTECTIVE COATING | 2019 |
|
RU2720171C1 |
BUILDING MORTAR | 2012 |
|
RU2485067C1 |
RAW MATERIAL MIXTURE FOR PROTECTIVE COATING | 2021 |
|
RU2762272C1 |
RAW MATERIAL MIXTURE | 2009 |
|
RU2396234C1 |
RAW MIX FOR PROTECTIVE COATING | 2016 |
|
RU2616948C1 |
RAW MIX FOR PROTECTIVE COATING | 2016 |
|
RU2616204C1 |
Authors
Dates
2018-12-13—Published
2018-02-01—Filed