FIELD: chemistry; manufacturing technology.
SUBSTANCE: invention relates to a rubber mixture, a pneumatic tire and a diaphragm for tire vulcanisation. Rubber mixture contains a rubber component containing 85 wt % or more in total amount of at least one rubber, selected from butyl rubber and halogenated butyl rubber, terpene-based resin, having glass transition temperature of 60 °C or less, 6–30 wt h in total amount of non-terpenic resin, having a glass transition temperature of 50 °C or more, different from terpene-based resin, having a glass transition temperature of 60 °C or less, per 100 wt h rubber component, as well as soot and sulfur.
EFFECT: invention provides excellent resistance to air penetration, moldability and durability of pneumatic tire and diaphragm for tire vulcanisation.
9 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
WINTER TIRE | 2016 |
|
RU2703207C1 |
PNEUMATIC TIRE | 2017 |
|
RU2699673C1 |
METHOD OF PRODUCING VULCANISED RUBBER MIXTURE, VULCANISED RUBBER MIXTURE AND STUDLESS TIRE MADE USING SAID RUBBER MIXTURE | 2015 |
|
RU2706665C2 |
TIRE | 2015 |
|
RU2614121C1 |
RUBBER MIXTURE FOR SIDE WALLS AND PNEUMATIC TYRE MADE FROM SAID MIXTURE | 2008 |
|
RU2458082C2 |
STUDLESS TIRE | 2018 |
|
RU2742878C1 |
RUBBER MIXTURE AND PNEUMATIC TYRE MADE FROM SAID MIXTURE | 2008 |
|
RU2468045C2 |
STUDDED TIRE AND RUBBER COMPOSITION FOR TIRES | 2018 |
|
RU2721443C1 |
RUBBER COMPOSITION FOR USE IN THE TIRE PROTECTOR | 2015 |
|
RU2627853C1 |
RUBBER MIXTURE FOR SIDEWALL REINFORCING LAYER OR FOR SIDEWALL AND TIRE | 2009 |
|
RU2520491C2 |
Authors
Dates
2020-03-25—Published
2016-07-25—Filed