FIELD: quantum electronics. SUBSTANCE: laser medium production process involves or radiation of lithium fluoride crystal doped with magnesium at temperature of 196 to 40 C and dosage rate of 108-109 R followed by its exposure to temperature of 90-100 C for 1.5-2 h. EFFECT: provision for generation in the range of 0.64 to 0.72 mcm, improved service life of laser in mentioned range. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING ACTIVE ELEMENT FOR LASER BASED ON FLUORIDE LITHIUM CRYSTAL WITH PAINTING CENTERS | 1983 |
|
SU1152475A1 |
METHOD OF MANUFACTURING LASER ENVIRONMENT FOR ACTIVE ELEMENTS AND PASSIVE GATES | 1981 |
|
SU1064835A1 |
PROCESS OF MANUFACTURE OF LASER ELEMENT | 1985 |
|
SU1331394A1 |
METHOD OF MANUFACTURING ACTIVE ELEMENT FOR SOLID LASER | 1979 |
|
SU814225A1 |
ACTIVE LASER MEDIUM ON BASE OF MONOCRYSTAL OF LITHIUM FLUORIDE FF COLOUR CENTERS AND PROCESS OF ITS PRODUCTION | 1985 |
|
SU1322948A1 |
LASER, LASER ACTIVE ELEMENT AND METHOD OF PRODUCING ACTIVE ELEMENTS | 1980 |
|
SU986268A1 |
MATERIAL FOR ACTIVE ELEMENTS OF LASERS, PASSIVE LASER GATES AND DIAPHRAGMS | 1982 |
|
SU1123499A1 |
LASER MATERIAL | 1986 |
|
SU1538846A1 |
METHOD OF MANUFACTURING OPTICAL MEMBERS FOR LASERS | 1981 |
|
SU1028100A1 |
ACTIVE MEDIUM OF LASER | 1986 |
|
SU1407368A1 |
Authors
Dates
1995-07-25—Published
1984-06-15—Filed