FIELD: alloys. SUBSTANCE: alloy has the following components, wt.-%: Co 12.5-40; Ni 10-16; Al 7-9; Ti 0.1-5; Cu 1-3.5; Hf 0.1-0.8; Nb 0.1-0.8; Mn 0.1-1.0; Si 0.1-1.0; S 0.2-0.3, and Fe - the rest. Alloy deoxidation with manganese, silicon and sulfur results in more complete deoxidation and purity by oxygen, nitrogen and nonmetallic inclusions. Negative effect of titanium is neutralized, polishing is improved, and formed sulfides act as lubricant. Alloy properties: Br = 8000-13000 Gs; Hc = 640-1800 E; (BH)max = 3.6-7.0 mln Gs x E; σ = 12000 - 20000 kg/cm2. EFFECT: increased magnetic properties of alloy. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ALLOY FOR PERMANENT MAGNETS | 1988 |
|
RU1612617C |
ALLOY FOR PERMANENT MAGNETS AND ITS PRODUCTION PROCESS | 1992 |
|
RU2061269C1 |
0 |
|
SU558961A1 | |
0 |
|
SU359278A1 | |
GRANULATED HIGH-TEMPERATURE NICKEL ALLOY AND PRODUCT MANUFACTURED THEREFROM | 2016 |
|
RU2623540C1 |
MAGNETIC ALLOY | 1990 |
|
RU2008736C1 |
COMPOSITION OF NICKEL-BASED HEAT-RESISTANT ALLOY CHARGE OF EQUIAXIAL STRUCTURE FOR GAS TURBINE WORKING BLADE CASTING | 2014 |
|
RU2562202C1 |
CORROSION-RESISTANT STEEL | 1991 |
|
RU2016133C1 |
ALLOY FOR PERMANENT MAGNETS | 2012 |
|
RU2510422C1 |
HEAT-RESISTANT NICKEL-BASED ALLOY FOR CASTING GAS TURBINE HOT SECTION PARTS OF PLANTS WITH EQUIAXIAL STRUCTURE | 2015 |
|
RU2581337C1 |
Authors
Dates
1995-04-20—Published
1984-03-07—Filed