FIELD: manufacture of absorbing materials. SUBSTANCE: copolymer of 2-methyl-5-vinylpyridine or 4-vinylpyridine, hydrolyzate of acrylonitrile, divinylbenzene and ethylsterene is used as ion exchanger, with their weight mixture ratio being of 16-49: 8-25: 16-47: 10-29, respectively. Process for manufacturing such complexing resin is characterized by copolymerization of vinylpyridine monomer, acrylonitrile, divinylbenzene and ethylsterene followed by hydrolytic oxidation of nitrilo groups with nitric acid solution. EFFECT: increased adsorptive capacity and selectivity of ion exchanger resin. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING EASILY REGENERATED IONITE | 2012 |
|
RU2493915C1 |
METHOD OF OBTAINING COMPLEX-FORMING IONITE WITH ANINOCARBOLIC ACID GROUPS | 0 |
|
SU679593A1 |
METHOD FOR ION EXCHANGER PREPARATION FOR GOLD SORPTION | 2016 |
|
RU2615522C1 |
PYRIDINE IONITE FOR SORBING URANIUM FROM SOLUTIONS AND PULP | 2008 |
|
RU2385885C1 |
METHOD OF OBTAINING IONITES | 0 |
|
SU471795A1 |
0 |
|
SU547455A1 | |
0 |
|
SU449917A1 | |
METHOD FOR OBTAINING ANIONITES | 0 |
|
SU1657513A1 |
0 |
|
SU531815A1 | |
METHOD OF PREPARING ANION-EXCHANGE RESINS | 0 |
|
SU689218A1 |
Authors
Dates
1994-02-28—Published
1986-06-04—Filed