FIELD: coal chemistry. SUBSTANCE: suspension has the following components, wt.-%: coal, 58-60; humate, 0.5-0.7; and water, up to 100. The source of humate is hydroxylamino-, alkylamino-, arylaminosulfohumates or a mixture of sodium humate with amines - urea, thiourea, tetraethylammonium chloride. This suspension exhibits the better stability (up to 20-25 days), decreased viscosity (up to 0.231-0.541 Pa x s). This suspension can be transported by pipe-line. EFFECT: improved property and quality of suspension. 2 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF THE WATER-METHOD FUEL AND ITS COMPOSITION | 2005 |
|
RU2277120C1 |
METHOD OF PREPARING CAVITATION WATER-COAL FUEL (CaVWCF) AND PROCESS LINE FOR IMPLEMENTATION OF THIS METHOD | 2006 |
|
RU2380399C2 |
METHOD FOR PRODUCING WATER-AND-CARBON SUSPENSION | 1990 |
|
SU1757228A1 |
WATER-COAL SLURRY | 0 |
|
SU1402606A1 |
METHOD OF PRODUCING ASH CEMENT | 2014 |
|
RU2543833C2 |
COAL-WATER SUSPENSION | 0 |
|
SU1545947A3 |
METHOD OF PRODUCING COAL WATER SUSPENSION | 0 |
|
SU1538901A3 |
METHOD FOR DECREASING DYNAMIC VISCOSITY OF WATER-COAL SUSPENSIONS | 2005 |
|
RU2297024C2 |
COAL-WATER SUSPENSION | 0 |
|
SU1554764A3 |
METHOD FOR PREPARATION OF WATER-BEARING FUEL-COAL SLURRY | 2016 |
|
RU2611630C1 |
Authors
Dates
1999-02-27—Published
1987-03-25—Filed