FIELD: photographic materials. SUBSTANCE: invention relates to photographic materials, in particular, to silver-free materials that can be used in reprography, photography, and when recording information by laser or oscillograph ray. To increase light sensitivity, light sensitive layer containing 64.5- 78.5 wt % polyvinyl alcohol and 13.7-18.0 wt % cupric chloride is supplemented with 7.4-19.4 wt % formaldehyde. EFFECT: increased light sensitivity by an order of magnitude. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PHOTOGRAPHIC MATERIAL | 1987 |
|
SU1441957A1 |
METHOD OF PRODUCING SILVERLESS IMAGE | 1983 |
|
SU1120833A1 |
METHOD OF PREPARING LIGHT SENSITIVE MATERIAL | 1982 |
|
SU1182901A1 |
METHOD OF PRODUCING SILVERLESS PHOTOGRAPHIC PICTURE | 0 |
|
SU1262440A1 |
METHOD OF PRODUCTION SILVERLESS PHOTOGRAPHIC MATERIAL | 1992 |
|
RU2006054C1 |
METHOD OF PRODUCING PHOTOGRAPHIC MATERIAL | 0 |
|
SU996983A1 |
LIGHT-SENSITIVE COMPOSITION FOR PRODUCING PHOTOGRAPHIC THERMODEVELOPING MATERIAL | 0 |
|
SU1097964A1 |
METHOD OF PRODUCING PICTURE ON LEAD IODIDE BASED LIGHT-SENSITIVE MATERIAL | 0 |
|
SU960716A1 |
LIGHT-SENSITIVE RECORDING MATERIAL | 2003 |
|
RU2302652C2 |
PHOTOCHROME MATERIAL | 1983 |
|
SU1194177A1 |
Authors
Dates
1998-04-27—Published
1987-08-05—Filed