FIELD: photographic material production. SUBSTANCE: sensitizer is solved in a low-boiling water immiscible organic solvent. Then the resultant solution is mixed with a polymer in the proportion of 1 to 5-10. The polymer is formulated as where R = H, CH3; n = 0.02-0.15; m = 0.98- 0.85. The polymer molecular mass is 2000-5000. Then the solution is dispersed in a 3% water-and-gelatin solution. The resulting composition is stable during up to 30 days. EFFECT: increased stability. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF MANUFACTURE OF BROMINE-IODINE-SILVER PHOTOGRAPHIC EMULSION AND PHOTOGRAPHIC MATERIAL BASED ON IT | 2002 |
|
RU2215316C1 |
SILVER HALIDE PHOTOGRAPHIC MATERIAL FOR MEDICAL RADIOGRAPHY | 2001 |
|
RU2195011C1 |
LATEX FOR PHOTOGRAPHIC MATERIAL MANUFACTURING | 1991 |
|
RU2009531C1 |
SILVER HALIDE PHOTOGRAPHIC MATERIAL | 2000 |
|
RU2184387C1 |
PHOTOGRAPHIC HALOGEN-SILVER SUBSTANCE | 1997 |
|
RU2125735C1 |
SILVER HALIDE PHOTOGRAPHIC MATERIAL | 1997 |
|
RU2126166C1 |
METHOD OF MANUFACTURING SILVER BROMIDE PHOTOGRAPHIC EMULSION | 2002 |
|
RU2224277C1 |
LATEXES OF COPOLYMERS OF BUTYLACRYLATE AND DI-N-SUBSTITUTED ACRYLAMIDE | 0 |
|
SU1819274A3 |
COMPOSITION OF SOLUTION OF HYDROPHOBIC COLOR-FORMING COMPONENTS | 1991 |
|
RU2026569C1 |
SILVER HALIDE PHOTOGRAPHIC MATERIAL | 2002 |
|
RU2206915C1 |
Authors
Dates
1994-05-15—Published
1989-09-25—Filed