FIELD: strengthening of oil and gas holes. SUBSTANCE: complex reagent has, wt. -%: hypan 7-8; 2-hydroxy-1,3-propylenediaminotetramethylphosphonic acid tetrasodium salt 3.5-4.0; sodium hydroxide 38-40, and water - the rest. Hypan and tetrasodium salt of 2-hydroxy-1,3-propylenediaminotetramethylphosphonic acid were taken at the ratio 2:1. EFFECT: increased safety of strengthening at raised and high temperatures. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPLEX REAGENT FOR PLUGGING LIQUIDS ON THE BASIS OF PORTLAND CEMENT | 1990 |
|
SU1839040A1 |
COMPLEX AGENT FOR CEMENTING COMPOSITION | 0 |
|
SU1451257A1 |
GAS-CEMENT GROUTING MORTAR | 2014 |
|
RU2552261C1 |
COMPLEX REAGENT FOR GROUTING MORTAR | 2018 |
|
RU2691224C1 |
COMPLEX WELL PLUGGING SLURRY TREATMENT AGENT | 1991 |
|
RU2013524C1 |
COMPLEX REAGENT FOR HIGH-TEMPERATURE GROUTING MORTARS | 2005 |
|
RU2298576C1 |
LIGHT-WEIGHT HEAT-RESISTANT GROUTING MATERIAL | 1992 |
|
RU2043481C1 |
COMPOSITION FOR PREPARING PLUGGING FLUID | 0 |
|
SU1105612A1 |
PLUGGING COMPOSITION | 0 |
|
SU991025A1 |
GROUTING MORTAR FOR REPAIR JOBS AND WELL LINING | 1992 |
|
RU2035585C1 |
Authors
Dates
1995-04-10—Published
1990-10-01—Filed