FIELD: manufacture of plastics. SUBSTANCE: composition contains the following components, % by weight: aniline phenol-formaldehyde resin 33.4-36.8; kaolin 60.7-64.4; calcium stearate 1,2-1.4 and magnesia 0.9-1.4. For preparation of composition starting materials are stirred in mixer for 40 min to obtain homogeneous mixture. The mixture is milled, ground and press- molded. Given are characteristic performances of the finished product. EFFECT: increased strength, electrical and wear resistance. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMERIC MOULDING COMPOSITION | 0 |
|
SU1733445A1 |
METHOD FOR MANUFACTURING GRANULATER GLASS-REINFORCED PHENOPLASTS BY UTILIZATION WASTE PRODUCTS OF PROPORTIONING GLASS-FIBER MATERIALS | 0 |
|
SU1678640A1 |
POLYMERIC COMPOSITION | 1995 |
|
RU2100390C1 |
POLYMERIC MOLDING COMPOSITION | 0 |
|
SU1797614A3 |
POLYMERIC MOULDING COMPOSITION | 0 |
|
SU1692998A1 |
POLYMER COMPOUND | 0 |
|
SU1675306A1 |
METHOD AND COMPLEX FOR CONTINUOUS PRODUCTION OF PHENOLIC PLASTICS | 0 |
|
SU1801752A1 |
COMPOSITION FOR PREPARING PRESSING COMPOUND | 2000 |
|
RU2198189C2 |
POLYMERIC CASTING COMPOSITION | 2003 |
|
RU2250913C1 |
COMPOSITION FOR FIRE-RESISTANT MATERIAL | 2002 |
|
RU2219203C2 |
Authors
Dates
1994-01-15—Published
1992-03-11—Filed