FIELD: synthetic leather finish. SUBSTANCE: polyesteruretane is dissolved in dimethyl formamide followed by addition of 13-20 % by weight of incontinuous hollow poly-4-methylpent-1-ene filament to the resulting solution prior to film-formation. The resulting mixture is applied to substrate material followed by film-forming in coagulating medium, washing and drying to obtain poromeric film material with percentage elongation 120-210, vapor permeability 1.3-2.0 mg/cm kW/h. EFFECT: high water vapor resistance. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER COMPOSITION FOR PREPARING FACE COATING OF ARTIFICIAL LEATHER | 2006 |
|
RU2303618C1 |
LAMINAR COMBINED MATERIAL | 2011 |
|
RU2482967C1 |
COMPOSITION FOR PRODUCING VAPOUR-PERMEABLE POROUS MEMBRANE | 2018 |
|
RU2688625C1 |
METHOD OF PRODUCING POROUS POLYMER MATERIAL | 0 |
|
SU1684293A1 |
COMBINED MATERIAL - LAMINATE | 2011 |
|
RU2473293C1 |
COMBINED MULTI-LAYER MATERIAL | 2009 |
|
RU2412625C1 |
POLYMER COMPOSITION FOR PREPARING FACE COATING OF ARTIFICIAL LEATHER | 2006 |
|
RU2303619C1 |
MULTI-LAYER HERMETIC ELASTIC COLD-RESISTANT MATERIAL OF ARTIFICIAL LEATHER TYPE | 2004 |
|
RU2265684C1 |
FIREPROOF DECORATIVE-FINISHING MATERIAL AND METHOD OF OBTAINING THEREOF | 2012 |
|
RU2523330C2 |
METHOD OF MANUFACTURING SIMULATED LEATHER | 1994 |
|
RU2074274C1 |
Authors
Dates
1994-01-15—Published
1992-06-09—Filed