FIELD: manufacture of thermoplastic elastomers. SUBSTANCE: composition contains 100 parts by weight of vynylsiloxane rubber, 20-160 parts by weight of block-copolymer of the general formula (C6H5SiO1.5)n[(CH3)2SiO]m, wherein n = 35-80; m= 70-300, having 0.1-1.0 % by weight of hydroxyl groups bonded with silicon atoms and 40-95 parts by weight. Characterization of finished products is as follows: thermal shrinkage ratio 1.2-1.9, tensile strength after air-ageing at 300 C for 72 hrs 3.0-5.0 MPa. EFFECT: high freezing and heat resistance. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
THERMOSTABLE COMPOSITE BASED ON SILOXANE BLOCK-COPOLYMER | 2000 |
|
RU2196154C2 |
FIREPROOF HEAT-PROTECTIVE MATERIAL | 2014 |
|
RU2559499C1 |
RUBBER MIXTURE | 1992 |
|
RU2010814C1 |
CERAMICS-FORMING RUBBER MIXTURE (VERSIONS) | 2012 |
|
RU2519379C2 |
RUBBER MIXTURE ON THE BASE OF ETHYLENE-PROPYLENE (DIENE) CAOUTCHOUC | 1994 |
|
RU2074205C1 |
POLYMERIC COMPOSITION | 1993 |
|
RU2068858C1 |
HEAT-SHIELDING POLYMERIC MATERIAL AND METHOD FOR ITS PREPARING | 2001 |
|
RU2220169C2 |
COMPOSITE FOR PRODUCTION OF GENERAL MECHANICAL RUBBER GOODS | 2004 |
|
RU2285703C2 |
PROCESS OF PRODUCTION OF ELECTRIC INSULATION COATING | 1990 |
|
RU2011233C1 |
COMPOSITE MATERIAL FOR PRODUCING COMPOSITE MATERIALS | 2013 |
|
RU2516500C1 |
Authors
Dates
1994-01-15—Published
1992-04-15—Filed