FIELD: rubber industry. SUBSTANCE: new rubber mixture includes 100 parts of polymer compound, 1.0 to 5.0 parts of curing agent, 1.0 to 5.0 parts of metal oxide, and 1.0 to 2.0 parts of organic compound to activate curing. Polymer compound further includes 60 to 80 parts of butadiene/methyl/styrene rubber, 20 to 40 parts of polyvinylchloride, and modified additive - 2,6-ditertbutyl-4-methylamino- dimethylphenol or 1.0 to 1.5 parts of poly/N-3,5-ditertbutyl-4- oxytolyl/ethylenimine. Rubber mixture may additionally contain 10 to 80 parts of filler. Thus prepared vulcanized rubber possess excellent physical- mechanical characteristics, namely: modulus of elasticity in 100-percent tension, relative tensile strength, elongation, hardness, fire-proofness and resistance to influence of ozone. EFFECT: better characteristics of rubber mixture. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2113445C1 |
THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2111985C1 |
METHOD OF PREPARING POLYMERIC AMINE ANTIOXIDANT | 1996 |
|
RU2130033C1 |
METHOD OF STABILIZING EMULSION-POLYMERIZATION RUBBERS | 1996 |
|
RU2123015C1 |
RUBBER COMPOUND | 1994 |
|
RU2083608C1 |
METHOD OF STABILIZATION OF EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130031C1 |
METHOD FOR PRODUCTION OF BUTADIENE-STYRENE(α-METHYL STYRENE) RUBBER BEING MODIFIED BY POLAR MONOMER | 1996 |
|
RU2115664C1 |
METHOD FOR FORMATION-AND-FINISHING OF BUTADIENE (METHYL)-STYRENE RUBBER FROM LATEX | 1989 |
|
RU2028305C1 |
BITUMEN COMPOSITION | 1995 |
|
RU2093538C1 |
0 |
|
SU1565727A1 |
Authors
Dates
1994-04-15—Published
1992-02-13—Filed