FIELD: production of electrodes for high-temperature electrochemical devices. SUBSTANCE: 0.5 M solution of manganese acetate ( its quantity being 22.6 ml ) is mixed with 0.5 M solution of lanthanum acetate ( its quantity being 13.3 ml ) and with 0.5 M solution of strontium acetate ( its quality is 9.0 ml ). 0.5 M solution of ammonia carbonate ( its quantity being 400 ml ) and 60 ml of hydrogen peroxide are added at pH 9.0. Thus prepared precipitate is sustained within 12 h and filtered. Then washing by distilled water and drying at 105 C within 6 h are carried out. Heat treatment at 1000 C is carried out within 2 h. EFFECT: decreases energy expense. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SYNTHESIS OF METAL MANGANITE | 1999 |
|
RU2186032C2 |
METHOD OF OBTAINING ZIRCONIUM DIOXIDE STABILIZED WITH CALCIUM OXIDE | 0 |
|
SU780412A1 |
METHOD OF OBTAINMENT OF SOLID OXIDE FUEL CELL WITH DOUBLE-LAYER CARRIER CATHODE | 2013 |
|
RU2523693C1 |
SOLID ELECTROLYTE | 0 |
|
SU1095567A1 |
REFRACTORY LIQUID | 1991 |
|
RU2062764C1 |
METHOD FOR PREPARING CATALYST OF METHANOL SYNTHESIS | 0 |
|
SU1126205A3 |
0 |
|
SU386846A1 | |
METHOD FOR PRODUCTION OF HEAT-RESISTANT CERAMIC PIGMENTS | 1991 |
|
RU2044013C1 |
REFRACTORY MASS FOR PROTECTING CARBORUNDUM HEATER | 0 |
|
SU769961A1 |
METHOD FOR PRODUCTION OF ALLOYED TITANIUM DIOXIDE | 1992 |
|
RU2043302C1 |
Authors
Dates
1994-01-30—Published
1991-10-25—Filed