FIELD: manufacture of wood fiber materials. SUBSTANCE: process includes the use of paper currency material to be shredded to fines of 40-50 ° as plant raw material and a flocculating agent, preferably 0.025-0.1 % aqueous solution of 1.2-dimethyl-5-vinyl-pyridinium-methyl sulfate, pH 6-9 as electrolyte. Formation and dehydration of fibrous structure is carried out in vacuum at pressure of 0.09 to 0.1 MPa and moisture content of 68-72 % with subsequent hot molding of it at temperature of 160 to 180 C, pressure of 0.5 to 2.5 MPa and 0.5-1 % moisture content of the end product. EFFECT: improved quality of wood fiber boards. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING TILES FROM PLANT RAW MATERIAL | 1991 |
|
RU2014217C1 |
METHOD OF FIBER-BOARD PRODUCTION | 2001 |
|
RU2177058C1 |
METHOD OF PRODUCING FIBREBOARD WITH REFINED SURFACE | 0 |
|
SU1527354A1 |
METHOD OF MAKING PARTICLE-BOARD IN MOIST PROCESS | 0 |
|
SU1381224A1 |
METHOD TO FABRICATE WOOD FIBER BOARDS WITH RELIEF PATTERN | 0 |
|
SU1721162A1 |
METHOD OR PREPARING MAT FOR MAKING FIBREBOARD | 0 |
|
SU1724773A1 |
METHOD OF MAKING THE PLATE MATERIAL OF VEGETABLE WASTE PRODUCTS | 1993 |
|
RU2034702C1 |
METHOD OF PRODUCING FIBREBOARD PANELS | 0 |
|
SU943367A1 |
FIBREBOARD MANUFACTURING PROCESS | 0 |
|
SU1472546A1 |
MIXTURE FOR MANUFACTURING FIBRE BOARDS | 0 |
|
SU1317005A1 |
Authors
Dates
1994-03-30—Published
1991-10-31—Filed