FIELD: plastic metal working. SUBSTANCE: initial solid blank is heated to the forging temperature. The central hole is formed by loosening and opening of the blank core subjected simultaneously to the effect of two pairs of strikers and arbor with piercing end piece. During this process the blank is rotated with the angle of turning between strikes equal to 13-15 deg and is fed in the direction of the strikers at a preset speed. Then the pipe is sized beginning from the same heating and on the same arbor without the piercing end piece. Device for realizing the method has arbor and two pairs of strikers mounted with the shift of their working surfaces along the axis of forging. Each pair of the strikers is adjusted to the preset size of compression and to ensuring the total degree of compression from 5 to 25 % . The arbor is provided with quick-detachable piercing end piece. EFFECT: extending operating capabilities. 3 cl, 7 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING HOLLOW CYLINDRICAL BILLETS FOR THICK-WALLED TUBES | 1993 |
|
RU2049590C1 |
METHOD OF MAKING PRECISION PIPES AND RADIAL FORGING MACHINE TO THIS END | 2011 |
|
RU2493931C2 |
METHOD AND RADIALLY FORGING MACHINE FOR PRODUCTION OF PRECISION PIPES | 1995 |
|
RU2070464C1 |
METHOD FOR MAKING PRESION ELONGATED CYLINDRICAL PRODUCTS, MAINLY BIMETALLIC ONES AND TOOL FOR PERFORMING THE SAME | 2003 |
|
RU2248260C1 |
METHOD OFF MAKING HOLLOW CYLINDRICAL BLANKS | 1990 |
|
RU2083310C1 |
METHOD OF MANUFACTURE OF FORGINGS, PREDOMINANTLY OUT OF METALS AND ALLOYS OF TITANIUM SUBGROUP AND FORGING COMPLEX FOR PERFORMING THE SAME | 2002 |
|
RU2220020C1 |
METHOD OF FORGING HOLLOW PARTS AND FORGING COMPLEX TO THIS END | 2011 |
|
RU2486985C2 |
PRODUCTION OF THIN-WALL PIPES OF HIGHER PRECISION FROM ALLOYED COPPER-BASED STRAIN-HARDENED ALLOYS | 2012 |
|
RU2539799C2 |
METHOD FOR MANUFACTURING OF FORGED PIECES | 2004 |
|
RU2284874C2 |
METHOD OF PRODUCING HOLLOW FORGINGS | 2009 |
|
RU2421295C1 |
Authors
Dates
1994-04-15—Published
1992-05-19—Filed