FIELD: mechanical engineering. SUBSTANCE: method involves removing access plugs from cylinder heads, annealing in a furnace at a limited temperature (520 C), shot-blasting internal cavity with a jet of intact cast iron shot 1.5-3.5 mm in size at the rate of not less than 15 m/s through holes, then washing said cavity. EFFECT: higher efficiency.
Authors
Dates
1994-04-30—Published
1991-12-23—Filed