FIELD: metal-working. SUBSTANCE: alloyed constructional steel castings were heated in vacuum furnace during 1 to 3 h at vacuum of 10-4mm Hg mm Hg and then allowed to cool in three steps, first, in vacuum heat-treatment furnace chamber to Ac1-(80-100)°C (80 to 100) C at cooling rate of 400 to 430 C/h, then in furnace cooling chamber to point of 200 C and finally in the air. EFFECT: more effective treatment. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF WELDING WIRE TREATMENT | 0 |
|
SU1691028A1 |
ALLOYED STEEL, HOLDER OR PART OF HOLDER FOR TOOL FOR PLASTIC MOULDING, STRENGTHENED WITH QUENCHING WORK PIECE FOR HOLDER OR PART OF HOLDER, PROCEDURE FOR PRODUCTION OF ALLOYED STEEL | 2007 |
|
RU2425170C2 |
NATURAL AND NON-TEMPERED ROUND STEEL WITH HIGH STRENGTH, HIGH IMPACT STRENGTH, EASE OF CUTTING AND METHOD OF ITS PRODUCTION | 2022 |
|
RU2822732C1 |
HIGH-STRENGTH STEEL HAVING HIGH DEFORMABILITY, AND METHOD OF PRODUCING SUCH STEEL | 2017 |
|
RU2712591C1 |
METHOD OF THERMAL TREATMENT OF ALLOY STRUCTURAL STEEL BILLETS | 0 |
|
SU881133A1 |
NODULAR CAST IRON, EUTECTIC CEMENTITE INCLUSIONS AND BAINITE-AUSTENITIC METAL BASE HEAT TREATMENT METHOD | 2018 |
|
RU2681076C1 |
BLANK OF CONSTRUCTION STEEL SUITABLE FOR WELDING AND METHOD FOR MAKING IT | 2003 |
|
RU2321668C2 |
TUBULAR ARTICLE HEAT TREATMENT PROCESS | 2004 |
|
RU2279487C1 |
METHOD OF THERMAL TREATING OF BILLETS | 0 |
|
SU1617011A1 |
METHOD OF STEEL BLANK HEAT TREATMENT | 2012 |
|
RU2532874C2 |
Authors
Dates
1994-04-30—Published
1991-02-15—Filed