FIELD: individual protective means. SUBSTANCE: the method consists in hot rolling, cooling, annealing, mechanical treatment, cold forming, quenching, tempering. Rolling is accomplished within a temperature range from Ac3 to Az3 with partial reductions within 12 to 14%. Annealing is carried out with utilization of rolling heat, quenching - at a rate of cooling within 40 to 50 C, and tempering - at a temperature of 140 to 170 C. EFFECT: facilitated procedure.
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF MANUFACTURE OF STEEL MONOSHEET ARMORED MEMBERS B 100 ST | 1999 | 
 | RU2139357C1 | 
| BULLETPROOF HETEROGENEOUS ARMOR OF ALLOYED STEEL FOR MEANS OF PERSONAL PROTECTION AND METHOD OF ITS PRODUCTION | 1994 | 
 | RU2090828C1 | 
| SHEET STEEL FOR ARMOUR PROTECTION | 2020 | 
 | RU2806620C2 | 
| ARMOR STEEL | 2003 | 
 | RU2236482C1 | 
| STRUCTURAL STEEL | 0 | 
 | SU1700091A1 | 
| SUPER-STRENGTH MULTI-PHASE STEEL AND METHOD FOR MAKING STEEL STRIP OF MULTI-PHASE STEEL | 2018 | 
 | RU2742998C1 | 
Authors
Dates
1994-06-30—Published
1992-07-30—Filed