FIELD: chemistry, technological processes.
SUBSTANCE: in water suspension of caolin solutions of acidified aluminium sulfate and powder-like starch or carboxymethylcellulise in amount 2-3% wt are introduced. Amount of caolin in mixture is 75-85% wt. Amount of produced synthetic alumosilicate in mixture is 15-25% wt. Suspension is subjected to dispersive drying at temperature 350°C. Dry microspherical granules are calcinated. Then calcinated granules are crystallised in alkaline aluminate solution. Crystallised microspherical zeolite of A type is washed with water from excessive alkali and dried.
EFFECT: zeolite granules have high wear resistance, phase frequency and adsorption capacity.
2 tbl, 3 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF OBTAINING MICROSPHERICAL ZEOLITE OF A TYPE WITH HIGH PHASE PURITY | 2007 | 
 | RU2336229C1 | 
| METHOD OF PRODUCING GRANULAR ZEOLITE MATERIAL NOT CONTAINING BINDER | 2009 | 
 | RU2425801C2 | 
| METHOD OF PRODUCING HIGH PHASE PURITY ZEOLITE A GRANULATED WITHOUT BINDER | 2009 | 
 | RU2420456C1 | 
| METHOD OF PRODUCING TYPE ZSM SUPERHIGH-SILICA MICROSPHERICAL ZEOLITE WITHOUT BINDER | 0 | 
 | SU1640111A1 | 
| METHOD OF PRODUCING HIGH PHASE PURITY ZEOLITE ADSORBENT OF STRUCTURE A AND X, GRANULATED WITHOUT BINDER | 2009 | 
 | RU2420457C1 | 
| METHOD FOR PRODUCING NAA GRANULATED ZEOLITE ADSORBENT | 2017 | 
 | RU2655104C1 | 
| METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 | 
 | RU2230779C1 | 
| METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITES | 2005 | 
 | RU2283279C1 | 
| METHOD OF PRODUCTION OF GRANULATED SYNTHETIC ZEOLITE-CONTAINING COMPONENT OF SYNTHETIC DETERGENTS | 2007 | 
 | RU2335534C1 | 
| METHOD OF PRODUCING GRANULAR SYNTHETIC TYPE A ZEOLITE | 2012 | 
 | RU2498939C1 | 
Authors
Dates
2008-10-27—Published
2007-04-16—Filed