FIELD: glass industry. SUBSTANCE: opaque glass has, wt.-%: silicon oxide (SiO2) 61.05-63.66; aluminium oxide (Al2O3) 0.86-0.92; calcium oxide (CaO) 9.18-9.94; potassium oxide (K2O) 4.45-4.63; sodium oxide (Na2O) 14.59-15.23; arsenic oxide (As2O3) 0.27-0.29; phosphorus pentoxide (P2O5) 2.5-5.4; fluoride (F′) 0.98-1; barium oxide (BaO) 2.18-2.28, and antimony oxide (Sb2O3) 0.27-0.29. Making temperature is 1370-1380 C, caking point is 910-920 C. Glass is used for making of facing materials. EFFECT: enhanced quality of glass. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
BLACK GLASS | 1991 |
|
RU2016858C1 |
OPTICAL GLASS | 1993 |
|
RU2049745C1 |
GLASS FOR DARK-RED GLASS-CRYSTALLINE MATERIAL WHICH IS TRANSPARENT IN INFRARED REGION OF SPECTRA | 1990 |
|
RU2032633C1 |
OPAQUE GLASS | 1992 |
|
RU2045486C1 |
ELECTROVACUUM GLASS | 1995 |
|
RU2108987C1 |
OPTIC GLASS | 1993 |
|
RU2036172C1 |
GLASS FOR MICROCHANNEL AMPLIFIERS | 1994 |
|
RU2087436C1 |
AVENTURINE GLASS | 1991 |
|
RU2020135C1 |
GLAZE | 1991 |
|
RU2024446C1 |
GLASS | 1991 |
|
RU2016856C1 |
Authors
Dates
1994-07-30—Published
1991-04-23—Filed