FIELD: chemical technology. SUBSTANCE: carbon-containing material is carbonized at 400-600 C, heated without gaseous reagents up to 800-850 C at the rate of temperature increase 50-100 C/h, activated by steam at the mass ratio of carbon-containing material and steam = 1:5-10 and milled. EFFECT: improved method of activated carbon making. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ACTIVE COAL | 1993 |
|
RU2049054C1 |
METHOD OF ACTIVATED CARBON PRODUCING | 1993 |
|
RU2023663C1 |
METHOD OF PRODUCING CARBON FIBROUS ADSORBENT | 1992 |
|
RU2049168C1 |
METHOD OF MANUFACTURING ACTIVE CARBON | 0 |
|
SU1836289A3 |
METHOD OF PRODUCING ACTIVATED CHARCOAL FROM PLANT WASTES | 2013 |
|
RU2527221C1 |
METHOD FOR PRODUCTION OF ACTIVATED CARBON | 1993 |
|
RU2057067C1 |
METHOD OF CHARCOAL PREPARING | 1993 |
|
RU2031837C1 |
POWDERED ACTIVATED CARBON PRODUCTION PROCESS | 1999 |
|
RU2154605C1 |
METHOD FOR PRODUCTION OF ACTIVE COAL OF FRUIT KERNEL AND NUT SHELL | 1997 |
|
RU2111923C1 |
METHOD OF PREPARING ACTIVATED CARBON | 1995 |
|
RU2083491C1 |
Authors
Dates
1994-11-30—Published
1993-07-27—Filed