FIELD: building materials. SUBSTANCE: complex antifrosty additive has, wt. -% : sodium nitrite 32-50; waste of ferrosilicon production 49-65, and potash 1-3. Concrete compression strength with additive (after 24 h hardening at negative temperature) is up to 2,75 MPa, bending strength is up to 1.14 MPa, resistance to cold is up to 450 cycles. Compression strength of concrete with additive (after 24 h hardening at negative temperature and TBO) is 40.9 MPa, bending strength is 8.6 MPa. Complex additive is used in concrete for working at the winter conditions. EFFECT: enhanced quality of complex additive. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PRECAST REINFORCED CONCRETE PIECES PRODUCTION METHOD | 1991 |
|
RU2036188C1 |
COMPLEX ADDITIVE FOR CONCRETE MIXES AND MORTARS | 2006 |
|
RU2308429C1 |
COMPLEX ADDITIVE FOR CONCRETE, MORTAR AND CEMENT COMPOSITES (VERSIONS) AND METHOD OF PRODUCING SAID ADDITIVE | 2011 |
|
RU2467968C1 |
COMPLEX ANTIFREEZE ADDITIVE FOR CONCRETE AND MORTAR | 2012 |
|
RU2494987C1 |
COMPLEX ADDITIVE | 2004 |
|
RU2273613C2 |
COMPLEX ADDITIVE TO CONCRETE MIX | 0 |
|
SU638563A1 |
ANTIFREEZE ADDITIVE FOR CONCRETE MIXTURE | 2019 |
|
RU2728023C1 |
METHOD OF MANUFACTURE OF CONCRETE AND REINFORCED CONCRETE ARTICLES | 2006 |
|
RU2319681C1 |
RAW MIXTURE AND METHOD OF MANUFACTURING FLAT AND CORRUGATED SHEET THEREFROM | 2008 |
|
RU2369576C1 |
CONCRETE COMPOSITION AND PROCESSES FOR PREPARATION THEREOF | 1995 |
|
RU2067564C1 |
Authors
Dates
1994-12-15—Published
1991-07-19—Filed