FIELD: processes for the preparation of a polymeric material. SUBSTANCE: the process for preparing a foaming polymeric material comprises dissolving 100 wt parts of paraform (formaldehyde) in 200 wt parts of a 0.5% NaOH solution under stirring to 40-60 C for 30-40 minutes. 110-140 wt parts of dicyanodiamide are then added under continuous stirring and the dicyanodiamide are then added under continuous stirring and the mixture is kept for 40-60 minutes. 90-130 wt parts of xylite backflow are then poured and the whole mixture is heated for another 100-120 minutes. 40-100 wt parts of orthophosphoric acid are added and the process is continued under stirring for 50-70 minutes. The resulting product is thereafter dried at 120-150 C for 6-8 hr. EFFECT: improved proper ties of the polymeric material. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR PREPARING FOAMING POLYMERIC ANTIPYRENE | 1991 |
|
RU2026310C1 |
FIREPROOFING COMPOSITION FOR COATING OF METALLIC CONSTRUCTIONS | 1990 |
|
RU1804082C |
METHOD OF OBTAINING ANION EXCHANGER | 0 |
|
SU1015653A1 |
CELLULAR COMPOSITION FOR FIREPROOFING COVERING | 2000 |
|
RU2190649C2 |
FIRE-RETARDANT COMPOSITION FOR METAL STRUCTURE COATINGS | 1999 |
|
RU2185408C2 |
METHOD OF PREPARING FIREPROOFING COMPOUND | 2000 |
|
RU2172242C1 |
FIRE-PROTECTIVE FOAMING COMPOSITION FOR CONTAINING METALLIC CONSTRUCTIONS | 2001 |
|
RU2199564C1 |
FIRE-PROTECTIVE POLYMERIC COMPOSITION | 2015 |
|
RU2612720C1 |
METHOD OF MAKING FIREPROOF COATING FOR FIBRE-GLASS | 2012 |
|
RU2494129C1 |
METHOD OF MAKING FIREPROOF COATING FOR FIBRE-GLASS | 2013 |
|
RU2507231C1 |
Authors
Dates
1995-01-09—Published
1991-06-28—Filed