FIELD: building. SUBSTANCE: composition containing building gypsum and water has additionally ash, cement and boric acid at the water-solid ratio 0.5-0.57 at the following ratio of components, wt.-%: building gypsum 44.6-53.3; ash 8.7-10.8; cement 4.3-8.15; boric acid 0.1-0.3, and water - the rest. Strength of composition after 28 days is 130 kg/kg/cm2. EFFECT: enhanced quality of composition. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION GYPSUM MATERIAL | 1991 |
|
RU2017699C1 |
METHOD OF DETERMINATION OF PACKABILITY OF CEMENT-SAND MIXTURE | 1991 |
|
RU2015511C1 |
FEEDSTOCK MIXTURE FOR PRODUCTION OF MINERAL FIBERS | 1991 |
|
RU2014301C1 |
COMPOSITE MATERIAL | 1991 |
|
RU2038336C1 |
METHOD FOR REINFORCING OF PIT WALL | 1991 |
|
RU2019627C1 |
LIGHT CONCRETE PREPARING METHOD | 1991 |
|
RU2013421C1 |
METHOD FOR MANUFACTURING TWO-LAYER BOARDS WITH PROTECTIVE-DECORATIVE COATING | 1990 |
|
RU2007294C1 |
METHOD FOR DETERMINING COMPOSITION OF CONCRETE MIX | 0 |
|
SU1762237A1 |
METHOD FOR PRODUCTION OF MINERAL FIBERS | 1991 |
|
RU2035409C1 |
POLYMERIC-CONCRETE MIX | 0 |
|
SU1776648A1 |
Authors
Dates
1995-01-20—Published
1991-05-27—Filed