FIELD: metallurgy. SUBSTANCE: scandium fluoride before its reduction is sublimated or distilled in vacuum or inert atmosphere at 800-1500 C. Condensate is cooled and ground. Prior to sublimation or distillation, scandium fluoride is mixed with calcium fluoride taken in the amount of 5-60% of mass of scandium fluoride. EFFECT: higher efficiency. 2 cl, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR PRODUCTION OF HIGH-PURITY METALLIC SCANDIUM | 1992 |
|
RU2034079C1 |
| METHOD OF METALLIC SCANDIUM PREPARING | 1992 |
|
RU2034078C1 |
| METHOD FOR PRODUCTION OF HIGH-PURITY METALLIC SCANDIUM | 1992 |
|
RU2034080C1 |
| METHOD FOR PRODUCTION OF HIGH-PURITY METALLIC SCANDIUM | 1992 |
|
RU2034077C1 |
| METHOD OF METALLIC SCANDIUM PREPARING | 1992 |
|
RU2034071C1 |
| METHOD OF HIGH PURITY SCANDIUM PREPARING | 1992 |
|
RU2034075C1 |
| METHOD FOR PRODUCTION OF METALLIC SCANDIUM | 1992 |
|
RU2034076C1 |
| METHOD FOR PRODUCTION OF METALLIC SCANDIUM | 1992 |
|
RU2034073C1 |
| METHOD FOR PREPARATION OF RARE-EARTH METAL-IRON ALLOYS FOR PERMANENT MAGNET | 0 |
|
SU1724712A1 |
| PROCESS OF PRODUCTION OF ALLOYS BASED ON RARE-EARTH METALS, SCANDIUM AND YTTRIUM | 1994 |
|
RU2061078C1 |
Authors
Dates
1995-04-30—Published
1992-01-28—Filed