FIELD: metallurgy of rare metals. SUBSTANCE: method includes distillation of crude metal in vacuum of 10-4-10 -5 mm Hg at temperature of 1650-1750 C. After condensation, distillation is repeated at temperature of 1850-2000 C. EFFECT: higher efficiency. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR PRODUCTION OF HIGH-PURITY METALLIC SCANDIUM | 1992 |
|
RU2034079C1 |
| METHOD OF HIGH PURITY SCANDIUM PREPARING | 1992 |
|
RU2034075C1 |
| METHOD FOR PRODUCTION OF HIGH-PURITY METALLIC SCANDIUM | 1992 |
|
RU2034077C1 |
| METHOD FOR PRODUCING HIGH-PURITY METAL SCANDIUM | 2020 |
|
RU2748846C1 |
| METHOD FOR PRODUCTION OF METALLIC SCANDIUM | 1992 |
|
RU2034072C1 |
| METHOD OF METALLIC SCANDIUM PREPARING | 1992 |
|
RU2034071C1 |
| METHOD FOR PRODUCTION OF METALLIC SCANDIUM | 1992 |
|
RU2034076C1 |
| METHOD OF METALLIC SCANDIUM PREPARING | 1992 |
|
RU2034078C1 |
| METHOD OF PRODUCTION OF SUPERALLOYS BASED ON NICKEL AND ALLOYED BY RARE-EARTH METALS | 2014 |
|
RU2572117C1 |
| METHOD FOR METAL OR SILICON RECEIVING | 2006 |
|
RU2339710C2 |
Authors
Dates
1995-04-30—Published
1992-01-28—Filed