FIELD: building materials. SUBSTANCE: raw mixture has, wt.-%: phosphogypsum (as dry dihydrate) 30-35; phosphosemihydrate (as dry semihydrate) 40-45, and cement dust - the rest. Compression strength of lumped phosphogypsum at the early time of hardening is 2.0-2.4, and water resistance is 78-79.4%. EFFECT: enhanced quality of material. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR GYPSUM ARTICLE MAKING | 1991 |
|
RU2028989C1 |
METHOD OF THE GRANULATED PHOSPHOGYPSUM MAKING | 1992 |
|
RU2087420C1 |
METHOD OF PRODUCING ANHYDRITE BINDER | 0 |
|
SU1730072A1 |
SULFIDIZER FOR PROCESSING OXIDIZED NON-FERROUS ORES AND CONCENTRATES | 0 |
|
SU1122726A1 |
METHOD OF CALCIUM SULPHATE PHOSPHOSEMIHYDRATE PROCESSING | 2009 |
|
RU2396209C1 |
METHOD OF PRODUCING GYPSUM BINDER, MODIFIED COMPOSITE GYPSUM BINDER AND METHOD FOR PRODUCTION THEREOF | 2015 |
|
RU2601962C1 |
ACTIVE MINERAL ADDITIVE FOR CEMENT AND METHOD FOR PREPARATION THEREOF | 2015 |
|
RU2581437C1 |
CONCRETE MIXTURE WITH HIGH EFFLORESCENCE RESISTANCE | 2017 |
|
RU2651683C1 |
RAW MIXTURE FOR PRODUCING PORTLAND CEMENT CLINKER | 0 |
|
SU1165659A1 |
SULPHOALUMINATE CLINKER WITH HIGH BELITE CONTENT, METHOD FOR ITS PREPARATION AND ITS APPLICATION FOR HYDRAULIC BINDERS | 2005 |
|
RU2360874C2 |
Authors
Dates
1995-05-10—Published
1991-10-28—Filed