FIELD: industry of building materials. SUBSTANCE: raw mixture has, wt. -% : portland cement 5-10; CaCO3 10-15; K2SO4 5-10; CaOSiO2 2-4; CaO x Fe2O3 1-3; dehydrated clay 1-3, and phosphorus semihydrate - the rest. Strength of freshly formed articles is 1.5 MPa. EFFECT: enhanced quality of articles. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| RAW MIXTURE FOR LUMPED PHOSPHOGYPSUM PRODUCING | 1991 |
|
RU2034805C1 |
| METHOD OF THE GRANULATED PHOSPHOGYPSUM MAKING | 1992 |
|
RU2087420C1 |
| METHOD OF PRODUCING ANHYDRITE BINDER | 0 |
|
SU1730072A1 |
| ACTIVE MINERAL ADDITIVE FOR CEMENT AND METHOD FOR PREPARATION THEREOF | 2015 |
|
RU2581437C1 |
| RAW MIXTURE FOR BUILDING MATERIAL MAKING | 1992 |
|
RU2062767C1 |
| COMPOSITE WATER-RESISTANT GYPSUM BINDING AGENT | 2012 |
|
RU2505504C1 |
| BINDING AGENT | 2013 |
|
RU2540706C1 |
| MIXTURE FOR AUTOCLAVE FOAM CONCRETE | 2011 |
|
RU2484066C1 |
| SULPHOALUMINATE CLINKER WITH HIGH BELITE CONTENT, METHOD FOR ITS PREPARATION AND ITS APPLICATION FOR HYDRAULIC BINDERS | 2005 |
|
RU2360874C2 |
| BINDER BASED ON INDUSTRIAL WASTES | 2023 |
|
RU2819999C1 |