FIELD: high-molecular compositions. SUBSTANCE: fireproofing polymeric composition has, mas. p.: ВПХ 100; ester plasticizer 45-52; lead stabilizing agent 4-6; antimony trioxide 4-9; aluminium hydroxide 10-30; aerosil 3-5, and epoxy resin 2-4. Material retains properties after exposition at 100 C for 7 days: resistance to cold and hardness retain at the parental levels - minus 45 C and 7-7.5 kgf/cm2, respectively. Retention of relative elongation after heat ageing is 98-99%. EFFECT: enhanced quality of composition. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER COMPOSITION | 1991 |
|
SU1832700A1 |
ELECTRICALLY INSULATING COMPOSITION | 2009 |
|
RU2402087C1 |
SUSPENSION POLYVINYL CHLORIDE COMPOSITION | 1988 |
|
SU1646278A1 |
ELECTRICALLY INSULATING COMPOSITION | 2011 |
|
RU2488608C1 |
ELECTRICALLY INSULATING COMPOSITION | 2009 |
|
RU2402085C1 |
INSULATING COMPOUND | 2001 |
|
RU2195729C1 |
ELECTRICALLY INSULATING COMPOSITION | 2009 |
|
RU2402086C1 |
ELECTRIC INSULATING COMPOSITION | 2005 |
|
RU2321911C2 |
ELECTRICALLY INSULATING COMPOSITION | 2010 |
|
RU2440632C1 |
FIREPROOF POLYMERIC COMPOSITION | 1998 |
|
RU2152410C1 |
Authors
Dates
1995-05-10—Published
1992-06-30—Filed