FIELD: chemical technology. SUBSTANCE: charge has the following components, wt.-%: calcium chloride 0.5-6; magnesium chloride hexahydrate (as anhydrous salt) 0.1-5, and purified calcium tungstate - the rest. Demineralized water, solution CaCl2 and solution MgCl2 were added to purified calcium tungstate, prepared charge is dried up to dusting state and calcined in air at 900 C for 1 h. Luminophore properties: relative intensity is 102-132%; relative post-luminescence is 14-99%; mean particle size is 3.8-5.0 mcm. EFFECT: enhanced quality of luminophore. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING CALCIUM TUNGSTATE X-RAY LUMINOPHOR | 2001 |
|
RU2209228C2 |
PROCESS OF SURFACE TREATMENT OF ZINC/CADMIUM SULFIDE-BASED LUMINOPHORES | 1991 |
|
RU2008318C1 |
IMAGE CONVERSION SCREEN MAKING METHOD | 1991 |
|
RU2008735C1 |
METHOD OF PRODUCING X-RAY PHOSPHOR GDOS:TB | 2019 |
|
RU2732140C1 |
PROCESS OF SURFACE TREATMENT OF ZINC/CADMIUM SULFIDE-BASED LUMINOPHORES | 1991 |
|
RU2008315C1 |
METHOD OF PRODUCING X-RAY PHOSPHOR BASED ON ZINC AND CADMIUM SULFIDES | 0 |
|
SU1490128A1 |
MULTI-ELEMENT X-RAY DETECTOR, RARE-EARTH X-RAY PHOSPHOR FOR SAID DETECTOR, METHOD OF MAKING MULTI-ELEMENT SCINTILLATOR AND DETECTOR ALTOGETHER | 2009 |
|
RU2420763C2 |
FAST-ACTING X-RAY-SENSITIVE PAD FOR DIGITAL MAMMOGRAPHY | 2012 |
|
RU2524449C2 |
METHOD OF PRODUCING X-RAY PHOSPHOR BASED ON ZINC OTHOPHOSPHATE, ACTIVATED WITH MANGANESE | 2015 |
|
RU2604619C1 |
METHOD OF LUMINOPHORE TREATMENT ON THE BASIS OF YTTRIUM COMPOUND ACTIVATED WITH LANTHANIDES | 0 |
|
SU1826982A3 |
Authors
Dates
1995-05-10—Published
1990-10-26—Filed