FIELD: chemical technology. SUBSTANCE: oxidized graphite powder is placed into closed gas-permeable form, heated at the rate 10-1000 C/s up to 350-550 C. Then article is annealed at the same temperature. EFFECT: improved method of graphite article making. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING LIGHT-WEIGHT PRODUCTS | 0 |
|
SU1054332A1 |
METHOD OF PRODUCING ULTRADISPERSED POWDER OF METALLIC IRON | 1992 |
|
RU2041026C1 |
METHOD FOR PRODUCTION OF FROTHED GRAPHITE | 1992 |
|
RU2057064C1 |
METHOD OF DETERMINING APPARENT DENSITY OF POROUS ARTICLES | 0 |
|
SU1820302A1 |
COMPOSITION FOR LINING DENTAL PROSTHESES | 1990 |
|
RU2045260C1 |
METHOD FOR PRODUCTION OF BIOSTIMULATING AGENTS | 1991 |
|
RU2014782C1 |
METHOD FOR TREATMENT OF MONOCRYSTALLINE ARTICLES FROM DISPERSED-SETTING MATERIALS | 1991 |
|
RU2033467C1 |
METHOD OF PREPARING OF BIOLOGICALLY ACTIVE AGENT ON THE BASIS OF BIRCH SAP | 1991 |
|
RU2019184C1 |
METHOD OF PRODUCING POROUS ISOTROPIC GRAPHITE MATERIALS | 1988 |
|
SU1617869A1 |
COMPOSITION FOR TEETH FILLING | 1994 |
|
RU2098077C1 |
Authors
Dates
1995-05-20—Published
1991-05-20—Filed