FIELD: powder engineering. SUBSTANCE: within this method hydroxy iron is dried at 80-100 C and pressure 11230-25270Pa, reduced at feeding speed 28-41 l/hour, temperature 250-400 C during 2-4 hours in pseudo-liquefied layer. Then hydroxy iron is immersed into 0,1-0,5 per cent oleic acid solution in hexane or decane, filtered, rinsed with hexane or decane and dried in the air. EFFECT: improved quality. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF PRODUCTION OF HIGH-DISPERSIVE IRON POWDERS AND OF IRON ALLOYS | 1991 |
|
RU2022060C1 |
MAGNETIC PIGMENT BASED ON MAGNETO-PERMEABLE CARBON BLACK, METHOD OF PREPARING SUCH CARBON BLACK, AND METHOD OF PREPARING MAGNETIC POWDER FOR MAGNETIC PIGMENT | 1995 |
|
RU2094172C1 |
METHOD OF PREPARING METAL MAGNETIC POWDER AND ALLOYS OF IRON GROUP | 1992 |
|
RU2041296C1 |
METHOD OF PREPARING FINE MAGNETIC POWDER | 1997 |
|
RU2118923C1 |
METHOD OF MAKING LIGHT-WEIGHT GRAPHITE ARTICLES | 1991 |
|
RU2035437C1 |
SUBSTANCE HAVING ADAPTATION PROMOTING ACTIVITY | 1992 |
|
RU2038085C1 |
METHOD FOR PRODUCTION OF BIOSTIMULATING AGENTS | 1991 |
|
RU2014782C1 |
METHOD OF PRODUCTION OF IRON-SILVER POWDER | 1995 |
|
RU2083331C1 |
METHOD OF OBTAINING MAGNET-CONTROLLED COMPOSITE MATERIAL | 0 |
|
SU1589327A1 |
METHOD OF MANUFACTURING OF MICROSPHERIC AEROSILOGEL | 0 |
|
SU1836292A3 |
Authors
Dates
1995-08-09—Published
1992-09-16—Filed