FIELD: paint and varnish industry. SUBSTANCE: priming material has, wt. -%: latex of butadiene-containing copolymer 52.3-52.8; carbamidoformaldehyde resin 3.8-4.7; sodium water glass after thermic working at 250-300 C for 2-3 h and milled up to dispersity 10-20 mcm 7.3-7.4; polyvinyl acetate dispersion 8.3-8.5; ethylsilicate 0.3-0.5; zinc white 6.6-6.9; chrome oxide 1.9-2.1; mica muscovite 6.3-7.9, and water - the rest. All components were stirred up to homogeneous mass, dispersed up to particle size 10-20 mcm and filtered. EFFECT: enhanced quality of priming material. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
AQUEOUS DISPERSIVE PAINT | 1996 |
|
RU2139309C1 |
GROUND COAT | 1992 |
|
RU2017776C1 |
METHOD OF PREPARING THE WATER-RESISTANT PHENOLFORMALDEHYDE FOAM PLASTIC | 1992 |
|
RU2085562C1 |
PROCESS FOR PREPARING PAINT-AND-VARNISH COMPOSITION | 0 |
|
SU1740393A1 |
RAW MATERIAL MIXTURE FOR MANUFACTURE OF HEAT-INSULATING MATERIAL AND METHOD OF PRODUCTION OF SUCH MIXTURE | 2001 |
|
RU2197448C1 |
RAW MIX FOR MANUFACTURING HEAT-INSULATING MATERIAL AND METHOD OF MANUFACTURING THEREOF | 1998 |
|
RU2148045C1 |
SILICATE PAINT | 2004 |
|
RU2272820C1 |
AN AQUEOUS-DISPERSION DYE | 1994 |
|
RU2109785C1 |
METHOD FOR PRODUCTION OF HEAT INSULATION AND FIRE RESISTANT COMBINED POLYMER COATING | 2007 |
|
RU2352601C2 |
VIBRATION-ABSORBING MASTICS | 1992 |
|
RU2043377C1 |
Authors
Dates
1995-05-27—Published
1992-07-31—Filed