FIELD: chemical technology. SUBSTANCE: semicoke having total volume of pores 0,20-0,40 см3/g, its ash content being 1.5-4.0 and content of phosphorous 0.6-1.2 is ground. Said semicoke is prepared on the base of cellulose or lignine being modified by 0.75-1.5 mass of orthophosphoric acid. Ground semicoke is mixed with binder and granulated. Thus prepared granules are dried, carbonized and affected by steam-gas activation till total content of pores is 0,60-0,75 см3/g. EFFECT: improves efficiency of the method. 5 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CHARCOAL PREPARING | 1993 |
|
RU2031837C1 |
METHOD OF ACTIVATED CARBON PRODUCING | 1993 |
|
RU2023663C1 |
METHOD OF PREPARING ACTIVATED CARBON | 1995 |
|
RU2083491C1 |
METHOD OF HEMOSORBENT PREPARING | 1991 |
|
RU2023503C1 |
METHOD FOR PRODUCTION OF ACTIVATED CARBON | 1993 |
|
RU2057067C1 |
METHOD TO CLEAR SEWAGE FROM PESTICIDES | 1993 |
|
RU2060961C1 |
METHOD FOR GASOLINE VAPORS RECOVERY IN MOTOR VEHICLE FUEL SYSTEM | 1992 |
|
RU2022626C1 |
METHOD OF PREPARING GRAINED ACTIVATED CARBON | 1990 |
|
RU2072319C1 |
METHOD OF PREPARING IMPREGNATED ADSORBENT | 1998 |
|
RU2133217C1 |
METHOD OF PREPARING MODIFIED ACTIVATED CARBON FOR MANUFACTURING CONDENSER ELECTRODES | 2000 |
|
RU2166478C1 |
Authors
Dates
1995-06-27—Published
1992-12-08—Filed