FIELD: alloys. SUBSTANCE: aluminium-base alloy has, wt.-% chrome 1.5-3.5; aluminium oxide 0.01-1.0; scandium 1.5-3.5; aluminium nitride 0.001-0.1, and aluminium the rest. Alloy properties: mechanical properties at 20 C: strength limit is 42-45 kg/cm,sq; creep limit is 36-39 kg/mm,sq; relative elongation is 14-16% at 350 C: strength limit is 16-18 kg/mm,sq; creep limit is 15-17 kg/mm, sq; relative elongation is 14-16% endurance limit at 350 C for 100 h is 8.0 kg/mm,sq. Alloy is used as structural material. EFFECT: enhanced quality of alloy. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ALUMINIUM-BASED ALLOY | 1994 |
|
RU2080406C1 |
DEFORMABLE THERMICALLY eNONHARDENED ALUMINIUM-BASE ALLOY | 1995 |
|
RU2082809C1 |
NICKEL-BASE ALLOY | 1992 |
|
RU2009244C1 |
HIGH-STRENGTH ALUMINIUM-BASED WROUGHT ALLOY OF Al-Zn-Mg-Cu-SYSTEM AND ARTICLE MADE THEREOF | 2015 |
|
RU2613270C1 |
NICKEL-BASE HEAT-RESISTANT ALLOY | 1997 |
|
RU2131943C1 |
ALUMINIUM-BASED WROUGHT AND THERMALLY NONSTRENGTHENABLE ALLOY | 1995 |
|
RU2081934C1 |
ANTIRUST ALLOY BASED ON Fe-Cr-Ni, ARTICLE THEREFROM AND METHOD OF PRODUCING SAID ARTICLE | 2010 |
|
RU2441089C1 |
ALUMINUM-BASED ALLOY | 2003 |
|
RU2251585C2 |
ALUMINIUM-BASE ALLOY FOR WELDING BY MELTING | 1995 |
|
RU2082808C1 |
NICKEL-BASE ALLOY | 1992 |
|
RU2017851C1 |
Authors
Dates
1995-06-27—Published
1993-06-24—Filed