FIELD: metallurgy. SUBSTANCE: alloy has the following components, wt.-% : carbon 0.03-0.08; chrome 9-11; tungsten 2.6-3.4; molybdenum 4.2-5.0; cobalt 11-13; titanium 2.6-3.4; aluminium 3.3-4.0; niobium 3.5-4.1; hafnium 0.1-3.0; boron 0.005-0.03; magnesium 0.002-0.05; lanthanum 0.005-0.03, and nickel - the rest. Ratio of chrome to cobalt content must be at the range 0.82-0.85. EFFECT: enhanced quality of alloy proposed. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
NICKEL-BASE ALLOY | 1992 |
|
RU2009244C1 |
NICKEL-BASE HEAT RESISTANT ALLOY | 1992 |
|
RU2022044C1 |
REFRACTORY NICKEL ALLOY FOR SINGLE-CRYSTAL CASTING AND PRODUCT MADE FROM THIS ALLOY | 2000 |
|
RU2186144C1 |
HEAT-RESISTANT NICKEL-BASE WROUGHT ALLOY AND ARTICLE MADE FROM THIS ALLOY | 2008 |
|
RU2365657C1 |
INTERMETALLIC ALLOY BASED ON NICKEL-ALUMINIUM-COBALT SYSTEM | 2015 |
|
RU2603415C1 |
HEAT-RESISTANT NICKEL-BASED ALLOY | 1999 |
|
RU2148100C1 |
POWDERED HEAT-RESISTANT ALLOYS FOR PRODUCING BIMETALLIC ARTICLES AND COMPOSITE DISC MADE OF THESE ALLOYS | 2016 |
|
RU2676121C2 |
HEAT-RESISTANT DEFORMED ALLOY ON BASE OF NICKEL AND ITEM MADE OF THIS ALLOY | 2014 |
|
RU2571674C1 |
SINTERED HEAT-RESISTANT NICKEL ALLOY | 2008 |
|
RU2368683C1 |
FIREPROOF POWDERED ALLOY BASED ON NICKEL RESISTANT TO SULFIDE CORROSION AND PRODUCT MADE FROM IT | 2013 |
|
RU2516681C1 |
Authors
Dates
1994-08-15—Published
1992-03-18—Filed