FIELD: metallurgy. SUBSTANCE: charge has calcium molybdate, reducing agent metallic calcium and molybdenum trioxide at the following ratio of components, wt. -% calcium molybdate 5.52-62.43; molybdenum trioxide 0.06-49.73, and metallic calcium 37.51-44.75. Invention ensures to obtain molybdenum in the form of spherical powder or ingot with high quality (as impurities content) at low cost. EFFECT: enhanced quality of charge. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RETORT LINING METHOD TO PRODUCE METALS BY METAL THERMAL REDUCTION SMELTING | 1992 |
|
RU2034058C1 |
METALLOTHERMIC PROCESS FOR EXTRACTING RARE-EARTH METALS FROM THEIR FLUORIDES FOR PRODUCING ALLOYS AND CHARGE FOR PERFORMING SUCH PROCESS | 2001 |
|
RU2181784C1 |
CHARGE FOR RECEIVING OF MOLYBDENUM | 2008 |
|
RU2367694C1 |
CHARGE FOR PRODUCING RARE-EARTH METALS | 1996 |
|
RU2103402C1 |
PROCESS FOR PREPARING CALCIUM MOLYBDATE | 1992 |
|
RU2049068C1 |
METHOD FOR THERMAL MELTING OF METAL | 2004 |
|
RU2269585C1 |
METHOD OF AUTOCLAVE PRODUCTION OF CHEMICALLY ACTIVE MATERIALS AND DEVICE TO THIS END | 2008 |
|
RU2405045C2 |
CHARGE FOR ALUMINIUM THERMAL PRODUCTION OF ADDITION ALLOYS WITH LOW ADDITIEVES CONTENTS | 2006 |
|
RU2331676C2 |
METHOD OF METAL URANIUM PRODUCTION | 2018 |
|
RU2681331C1 |
METHOD OF MELTING QUICK-CUTTING STEEL | 0 |
|