FIELD: metallurgy. SUBSTANCE: corrosion-resistant steel has components at the following ratio, wt.-% carbon 0.005-0.015; silicon 0.1-0.3; manganese 1.3-1.8; sulfur 0.005-0.015; phosphorus 0.005-0.015; chrome 17-18; nickel 13-14; copper 0.05-0.15; titanium 0.01-0.03; niobium 0.1-0.3; nitrogen 0.005-0.015; oxygen 0.001-0.005, cerium, scandium (in total) 0.01-0.06, and iron the rest. EFFECT: enhanced quality of steel. 4 tbl
Title | Year | Author | Number |
---|---|---|---|
CORROSION-RESISTANT STEEL | 1992 |
|
RU2016130C1 |
AUSTENITIC CORROSION-RESISTANT STEEL | 2002 |
|
RU2224045C1 |
AUSTENITIC HEAT-RESISTANT AND CORROSION-RESISTANT STEEL | 2015 |
|
RU2662512C2 |
STEEL | 1993 |
|
RU2063465C1 |
HIGH-STRENGTH LOW-MAGNETIC NON-STABILIZED WELDABLE STEEL, RESISTANT TO LOCAL CORROSION IN ZONES OF THERMAL AFFECT OF WELDING AND PROLONGED HEATING IN THE AREA OF HAZARDOUS TEMPERATURES | 2021 |
|
RU2782832C1 |
HEAT-RESISTANT AUSTENITIC STEEL | 2021 |
|
RU2781573C1 |
AUSTENITIC CORROSION-RESISTANT STEEL WITH NITROGEN | 2019 |
|
RU2716922C1 |
CORROSION-RESISTANT SCANDIUM ALLOY | 2022 |
|
RU2801911C1 |
UNSTABILIZED AUSTENITIC STEEL RESISTANT TO LOCAL CORROSION IN SCP-WATER | 2022 |
|
RU2790717C1 |
METHOD OF PRODUCING HOT-ROLLED COILS FROM COLD-RESISTANT AND CORROSION-RESISTANT STEEL | 2023 |
|
RU2813162C1 |
Authors
Dates
1995-07-09—Published
1993-03-10—Filed