FIELD: filler materials. SUBSTANCE: raw mixture has, wt.-% slag of heat power plant 70-75; clay 10-14; coal 1-2; lignin 1.5-3, and water the rest. Filler properties: compression strength is 1.8-2.2 MPa, filled density is 220-300 kg/m3. EFFECT: enhanced quality of porous filler. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR OBTAINING LIGHTWEIGHT AGGREGATE | 0 |
|
SU1555310A1 |
METHOD OF PRODUCING POROUS FILLER | 0 |
|
SU1482894A1 |
RAW MIXTURE FOR PRODUCING POROUS AGGREGATE | 0 |
|
SU1289845A1 |
RAW MIXTURE FOR MANUFACTURING POROUS FILLERS | 0 |
|
SU1555309A1 |
STARTING MATERIALS FOR PRODUCING LIGHT FILLER | 0 |
|
SU1625846A1 |
INITIAL MATERIAL MIXTURE FOR PRODUCING POROUS FILLER | 0 |
|
SU1404488A1 |
CRUDE MIXTURE FOR PRODUCING LIGHT AGGREGATE FOR CONCRETE (PENOZOL) | 2011 |
|
RU2479518C1 |
RAW MIXTURE FOR PRODUCING KERAMZIT | 0 |
|
SU1551682A1 |
RAW MATERIAL MIXTURE FOR MAKING LIGHTWEIGHT AGGREGATE | 0 |
|
SU1451121A1 |
METHOD OF LIGHT FILLING AGENT PRODUCING | 1995 |
|
RU2085529C1 |
Authors
Dates
1995-07-25—Published
1992-12-10—Filed