FIELD: nonferrous metallurgy. SUBSTANCE: sponge titanium is added on the melt surface together with ferroboron as a boron-containing compound. Then melt is covered with flux, and melt temperature is raised up to 850-900 C at the rate 3-5 C/min. EFFECT: improved method of master alloy preparing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF PRODUCING ALUMINUM-SILICON ALLOYS | 1991 |
|
RU2010881C1 |
METHOD OF REPROCESSING OF SILICON WASTE | 1991 |
|
RU2016110C1 |
METHOD OF REPROCESSING OF MAGNESIUM AND ITS ALLOYS WASTE | 1991 |
|
RU2010878C1 |
FLUXING AGENT FOR ALUMINUM AND ITS ALLOYS | 1992 |
|
RU2010882C1 |
METHOD FOR PRODUCTION OF ALUMINIUM ALLOY | 1993 |
|
RU2038398C1 |
METHOD OF PROTECTING LINING OF HEAT UNITS | 1992 |
|
RU2006372C1 |
METHOD OF PRODUCTION OF AN ALUMINIUM-TITANIUM ALLOYING COMPOSITION | 0 |
|
SU1836471A3 |
METHOD TO PRODUCE HYPEREUTETIC ALUMINUM-SILICON ALLOYS | 1993 |
|
RU2034927C1 |
METHOD FOR PRODUCTION OF HYPEREUTECTIC ALUMINUM-SILICON ALLOYS | 1993 |
|
RU2041967C1 |
METHOD OF PRODUCING ALLOYING COMPOSITION FOR MODIFYING ALUMINIUM ALLOYS | 0 |
|
SU1696551A1 |
Authors
Dates
1995-07-25—Published
1992-09-07—Filed