FIELD: technology of waste reprocessing. SUBSTANCE: magnesium or its alloys waste are added on the surface of melt containing 10-13.5% silicon at temperature 590-610 C. After increased up to 93-96% , flux consumption is decreased by 2.3% . EFFECT: improved method of reprocessing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF REPROCESSING OF SILICON WASTE | 1991 |
|
RU2016110C1 |
PROCESS OF PRODUCING ALUMINUM-SILICON ALLOYS | 1991 |
|
RU2010881C1 |
FLUXING AGENT FOR ALUMINUM AND ITS ALLOYS | 1992 |
|
RU2010882C1 |
METHOD OF CLEANING LADLES | 1995 |
|
RU2093608C1 |
METHOD OF PREPARING MASTER ALLOY ALUMINIUM-TITANIUM-BORON IN THE FURNACE | 1992 |
|
RU2040573C1 |
COMPOSITION FOR PROTECTING LINING OF HEAT ASSEMBLY | 1992 |
|
RU2093493C1 |
PROTECTIVE COATING FOR METAL SURFACES | 1995 |
|
RU2088368C1 |
METHOD FOR PRODUCTION OF SILUMIN | 1993 |
|
RU2065510C1 |
METHOD FOR PROCESSING OF ALUMINIUM ALLOY WASTE | 1990 |
|
RU2024637C1 |
METHOD OF PRODUCTION OF ALUMINUM ALLOY | 2001 |
|
RU2215803C2 |
Authors
Dates
1994-04-15—Published
1991-12-23—Filed