FIELD: refractory materials. SUBSTANCE: rammed mass has, wt.-% grained corundum 57-59; dispersed mixture of corundum and quartzite at their ratio (9.2-0.8): (8.8-1.2) 37-38; ortho-phosphoric acid 2-2.5, and binder as suspension of amorphized aluminosilicates and alumosol at the ratio (0.8-1.2): (1.2-0.8) 2-2.5, and binder has 15-20% of aluminium hydroxychloride. Properties: strength limit at mass compression after thermal working at 120 and 1500 C is 38-42 and 107-128 MPa, respectively, thermal stability is 1300 C; air above 55. EFFECT: enhanced quality of mass. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY BODY | 0 |
|
SU1719363A1 |
REFRACTORY COMPOSITION | 0 |
|
SU1049455A1 |
METHOD OF MAKING LINING FROM DRY TAMPING MASS | 0 |
|
SU1822490A3 |
REFRACTORY RAMMED MASS | 1991 |
|
RU2011648C1 |
REFRACTORY MASS FOR RAMMED LINING OF INDUCTION FURNACES | 1992 |
|
RU2068824C1 |
REFRACTORY MASS FOR RAMMED LINING | 1991 |
|
RU2011647C1 |
REFRACTORY PACKING MASS | 2003 |
|
RU2256631C1 |
STOCK FOR PRODUCING REFRACTORIES | 0 |
|
SU1738791A1 |
METHOD OF PRODUCING MULLITE-CORUNDUM REFRACTORY ARTICLES | 0 |
|
SU1347370A1 |
MULLITE-ROMEITE REFRACTORY MATERIAL | 1992 |
|
RU2040510C1 |
Authors
Dates
1995-08-09—Published
1992-02-17—Filed