FIELD: non-woven fabrics. SUBSTANCE: method involves applying binding layer to one side of canvas and drying it at 120-200 C to residual humidity of 10-15% Then the material is subjected to longitudinal stretching within the range of 10-20% The binding agent is applied to the canvas surface by spraying, to have up to 2-3% of overweight relative to canvas weight. EFFECT: improved strength and elasticity characteristics.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF NONWOVEN NEEDLE-PUNCHING MATERIAL REINFORCED WITH MESH | 2007 |
|
RU2360050C2 |
METHOD FOR MAKING NONWOVEN NEEDLED FELT | 2007 |
|
RU2345183C1 |
NEEDLE-PUNCHED FABRIC AND METHOD OF ITS PRODUCTION | 2007 |
|
RU2365687C1 |
METHOD FOR PRODUCING MATERIAL FOR SHOE INSOLE AND SUPINATOR AND MATERIAL FOR SHOE INSOLE AND SUPINATOR | 2002 |
|
RU2219815C1 |
OIL- AND OIL DERIVATIVE-GATHERING SORPTION MATERIAL AND METHOD OF MANUFACTURE THEREOF | 1997 |
|
RU2166362C2 |
NONWOVEN CARBONIC MATERIAL | 1996 |
|
RU2100500C1 |
BASE LAYER, METHOD FOR ITS PRODUCTION AND ITS USE | 2007 |
|
RU2456393C2 |
METHOD FOR PRODUCTION OF NONWOVEN BONDED MATERIAL | 1991 |
|
RU2057217C1 |
NON-WOVEN COMPOSITE LAMINATE | 2000 |
|
RU2248884C2 |
NON-WOVEN LAMINAR COMPOSITE MATERIAL AND A METHOD OF ITS PRODUCTION | 2000 |
|
RU2238851C2 |
Authors
Dates
1995-10-27—Published
1993-03-19—Filed