FIELD: polymeric compounds. SUBSTANCE: dispersion has polyvinylidene fluoride or copolymer 90-96 mol. vinylidene fluoride with 4-10 mol. tetrafluoroethylene and dispersion medium a mixture of ethanol or butanol and amide solvent and has additionally water at the following ratio of components, wt. -% polyvinylidene fluoride or copolymer 90-96 mol. vinylidene fluoride with 4-10 mol. tetrafluoroethylene 10-40; alcohol 32.0-58.1; amide solvent 18.5-35.6, and water 1.9-8.4. Mass ratio alcohol amide solvent 1:(0.5-0.7): (0.05-0.175). EFFECT: improved properties of dispersion. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING VINYLIDENE FLUORIDE- TETRAFLUOROETHYLENE COPOLYMERS | 1998 |
|
RU2139891C1 |
METHOD FOR PRODUCTION VINYLIDENE FLUORIDE-BASED POLYMERS | 2001 |
|
RU2200167C1 |
POROUS FLUOROCARBON MEMBRANE, METHOD OF ITS PREPARATION, AND CARTRIDGE FILTER BASED ON THIS MEMBRANE | 1995 |
|
RU2119817C1 |
METHOD OF PREPARING OF VINYLIDENE FLUORIDE WITH 5-12 MOL % OF HEXAFLUOROPROPYLENE | 1999 |
|
RU2164922C2 |
MODIFIED TETRAFLUOROETHYLENE/ETHYLENE COPOLYMER PRODUCTION PROCESS | 1999 |
|
RU2156776C1 |
COMPOSITION FOR PRODUCING POROUS MEMBRANE | 0 |
|
SU883100A1 |
PROCESS FOR PREPARING WEAK BASE ANION EXCHANGE MEMBRANE | 1991 |
|
RU2041892C1 |
PROCESS FOR PRODUCTION TETRAFLUOROETHYLENE COPOLYMERS WITH 2-5 MOL % OF PERFLUOROPROPYL VINYL ETHER | 1999 |
|
RU2156777C1 |
METHOD OF PRODUCING TETRAFLUOROETHYLENE COPOLYMERS WITH 12-15 MOL % OF HEXAFLUOROPROPYLENE | 1996 |
|
RU2109761C1 |
FLUORINATED POWDER MATERIAL FOR COATING APPLYING ON GALVANIZED STEEL AND COPOLYMERS OF VINYLIDENE FLUORIDE AS COMPONENT OF PIGMENTED POWDER MATERIALS | 1994 |
|
RU2119930C1 |
Authors
Dates
1995-11-10—Published
1982-07-02—Filed