FIELD: electroplating. SUBSTANCE: two layer deposition of zinc is exercised with pH of 4.8 5.6, temperature of 15 -40 C and current density of 0,5-5,0 A/dm2 from electrolyte with concentration, g/l, of: zinc salt 18 23 (in terms of metal), ammoniumchloride 180 200, boric acid 20 -25, polyethyleneglycol (ПЭГ-115) 5 8, sulfirol=8 1 2, and then, using the same mode, from electrolyte with concentration, g/l, of: zinc salt 29 34 ( in terms of metal), ammonium chloride 180 200, boric acid 20 25, gydropol=200 3 5, glycerin tar 5 8, sulfirol8 or СВ=105 12. EFFECT: improved quality of zinc coating. 2 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| BRIGHT-ZINC ELECTROLYTE | 0 | 
									
  | 
                SU655749A1 | 
| ELECTROLYTE FOR CATHODIC DEPOSITION OF CHROMITE CONVERSION FILMS | 0 | 
									
  | 
                SU1682412A1 | 
| ADDITIVE TO ZINC-PLATING ELECTROLYTES | 0 | 
									
  | 
                SU1177399A1 | 
| ELECTROLYTE FOR MIRROR-BRIGHT NICKEL PLATING | 0 | 
									
  | 
                SU1006546A1 | 
| ELECTROLYTE FOR NICKEL COATING APPLICATION | 0 | 
									
  | 
                SU1798386A1 | 
| ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-COBALT COATINGS | 2014 | 
									
  | 
                RU2569618C1 | 
| BRIGHT ZINC-PLATING ELECTROLYTE | 0 | 
									
  | 
                SU1439159A1 | 
| ELECTROLYTE FOR ELECTRODEPOSITION OF TIN-ZINC COATINGS | 2024 | 
									
  | 
                RU2840543C1 | 
| ELECTROLYTE FOR ELECTRODEPOSITION OF ZINC-NICKEL COATINGS | 2015 | 
									
  | 
                RU2603526C1 | 
| ELECTROLYTE FOR CATHODE CHROMATING OF ZINC | 0 | 
									
  | 
                SU1504291A1 | 
Authors
Dates
1995-11-20—Published
1990-07-17—Filed